Curved Wood

Solution Introduction

Curved wood craftsmanship, from replacing solid wood with materials, to solving the complex structure of furniture, to integrating into a series of home products. The application of curved wood has become mature, forming a unique and distinctive series of home products that are beautiful, generous, simple, and unique.

Curved wood craftsmanship: Cold pressing, hot pressing, and high-frequency processing techniques are used to integrate semi-finished curved wood products. Quality requirements: E1 formaldehyde emission level, E0 formaldehyde emission level, shaping, bonding strength (water boiling immersion peeling test). According to the requirements, IWG provides a comprehensive solution for system adhesive.


Integrated solution for curved wood adhesive:

E1 grade single component rubber powder

Hot pressing/high frequency:621 # formula adhesive

E1 grade dual liquid adhesive powder

Hot pressing/high frequency:605/602 formula adhesive

E0 grade modified urea formaldehyde resin adhesive

Hot pressing/high frequency:607 # formula adhesive

E0 grade formaldehyde free adhesive&curved wood assembly adhesive

Hot pressing/high frequency:SAP21360/PG186-1

Curved wood assembly adhesive:PG80/PG95


Common problem analysis

How to achieve a finished moisture content of less than 14% for multi-layer solid wood curved wood?

Process Control Standards

• The moisture content of solid wood veneer should be controlled at 6-8% before fabric bonding processing;

• The solid content of the adhesive application formula is greater than 75%;

• Double sided fabric adhesive, with a fabric adhesive content of 150-180g/m², single-sided fabric adhesive, with a fabric adhesive content of 120-140g/m²;

• Hot pressing temperature/time: 20mm thick plate, 105 ℃, hot pressing time 13-15 minutes;

• After the pressure relief, the formed board should be placed in a balanced dehumidification room for at least 72 hours before being sandblasted and coated.